Figure 6From: Influence of Anodic Conditions on Self-ordered Growth of Highly Aligned Titanium Oxide NanoporesX-ray diffraction patterns corresponding to: (a) as-received Ti foil; (b) Ti film anodized in HF (0.15 wt.%); (c) anodized in HF (0.5 wt.%) at RT; (d) anodized in HF (0.15 wt.%) at 2 °C; and (e) Ti film anodized in HF (0.15 wt.%) + H2SO4 (1 M) at RT. In all the cases the samples were anodized at 20 Vdc Back to article page