Figure 8From: Tunable Nanostructures and Crystal Structures in Titanium Oxide FilmsTEM bright field micrographs of different annealing conditions;a 1,100 °C—nanowires and fibrous grains and (b) 1200 °C—dendritic growth. Insets are SADPs froma rutile along [10] andb anatase along [001 zone axesBack to article page