Figure 6From: Preparation of Ultrafine Fe–Pt Alloy and Au Nanoparticle Colloids by KrF Excimer Laser Solution PhotolysisSize distributions of FePt nanoparticles with a precursor of Fe(III)(acac)3/Pt(II)(acac)2 = 2.4/0.6 mM (15 W, 300 mJ, 50 Hz) and that with a precursor of Fe(II)Cp2/Pt(II)(acac)2 = 4.0/6.0 mM (15 W, 300 mJ, 50 Hz)Back to article page