Table 1 Preparation conditions and morphology features of different samples
Sample | TBOT (mol/L) | PVP (g/L) | Diameter/thickness (nm) | Density (×1010 cm−2) |
---|---|---|---|---|
Nanodot-1 | 0.08 | 50 | 50 | 1.8 |
Nanodot-2 | 0.1 | 50 | 70 | 1.0 |
Film | 0.1 | – | 20 | – |
Sample | TBOT (mol/L) | PVP (g/L) | Diameter/thickness (nm) | Density (×1010 cm−2) |
---|---|---|---|---|
Nanodot-1 | 0.08 | 50 | 50 | 1.8 |
Nanodot-2 | 0.1 | 50 | 70 | 1.0 |
Film | 0.1 | – | 20 | – |