Figure 5From: The Modulation of Optical Property and its Correlation with Microstructures of ZnO Nanowiresa TEM image of ZnO nanowire annealed at 500 °C for 5 h in Ar and air mixed gas stream for 5 h,inset shows the SAED pattern of thecircled area in Fig. 5a;b HRTEM image ofcircled area in Fig. 5aBack to article page