Table 2 Lattice parameters, primitive cell volume, and transition temperature of samples A-D and MnAs bulk [27]
From: Strain-induced high ferromagnetic transition temperature of MnAs epilayer grown on GaAs (110)
MnAs bulk | Sample A | Sample B | Sample C | Sample D | |
---|---|---|---|---|---|
a (Å) | 5.71 | 5.78 | 5.71 | 5.67 | 5.69 |
b (Å) | 3.72 | 3.69 | 3.73 | 3.72 | 3.72 |
c (Å) | 6.45 | 6.41 | 6.43 | 6.45 | 6.45 |
T t (Å) | 313 | 325 | 335 | 350 | 350 |
V (Å3) | 137.06 | 136.71 | 136.95 | 136.05 | 136.53 |