Figure 1From: Grain size-dependent magnetic and electric properties in nanosized YMnO3 multiferroic ceramics The standard reference and the XRD patterns of YMnO 3 samples sintered at different temperatures. Samples were sintered at temperatures ranging from 800°C to 1,050°C for 2 h, respectively.Back to article page