Figure 3From: Grain size-dependent magnetic and electric properties in nanosized YMnO3 multiferroic ceramics The SEM micrographs for YMnO 3 samples. Samples sintered at (a) 800°C, (b) 850°C, (c) 900°C, and (d) 1,050°C, respectively.Back to article page