Table 1 Energy dispersive X-ray spectroscopy (EDX) analysis of top and bottom surface of TNP

From: Fabrication of complete titania nanoporous structures via electrochemical anodization of Ti

Element

Top

Bottom

 

wt%

at%

wt%

at%

C K

1.9

5.16

2.86

7.35

O K

14.92

30.49

19.04

36.71

F K

7.31

12.58

5.78

9.39

TiK

75.87

51.77

72.31

46.56

Total

100

100

100

100