Figure 1From: Photoluminescence of spray pyrolysis deposited ZnO nanorods XRD pattern of ZnO nanorod layer deposited by chemical spray pyrolysis. The layer was deposited onto ITO/SGL substrate at growth temperature of 550°C, using aqueous solution. SEM image of the corresponding ZnO nanorod sample is presented in Figure 3a.Back to article page