Figure 7From: Long-term oxidization and phase transition of InN nanotextures EDXS of film deposited on a Si substrate. The ratio of concentrations is (0.5InN/0.5In2O3) (a), and (0.3InN/0.7In2O3) (b) for 3 and 6 months exposure at ambient conditions, respectively.Back to article page