Table 1 Preparation conditions for different samples
From: Room-temperature nonequilibrium growth of controllable ZnO nanorod arrays
Zinc concentration (M) | R(molar ratio of Zn2+/OH-) | Medium volume (mL) | Sample Name |
---|---|---|---|
0.25 | 1:8 | 2 | A |
0.25 | 1:8 | 10 | B |
0.25 | 1:8 | 20 | C |
0.25 | 1:4 | 20 | D1 |
0.25 | 1:6 | 20 | D2 |
0.25 | 1:10 | 20 | D3 |
0.025 | 1:8 | 20 | E1 |
0.05 | 1:8 | 20 | E2 |
0.1 | 1:8 | 20 | E3 |