Table 1 Fitting results of the Raman spectra for various samples

From: Graphitic carbon growth on crystalline and amorphous oxide substrates using molecular beam epitaxy

Substrate

Peak (D) (cm−1)

Peak (G) (cm−1)

I D /I G

I 2D /I G

FWHM (G) (cm−1)

FWHM (2D) (cm−1)

SrTiO3

1,372

1,603

0.8

-

70

-

YSZ

1,364

1,609

1.1

-

63

-

SiO2

1,352

1,598

1.9

0.4

66

96

Glass

1,352

1,598

1.8

0.3

66

99

  1. Mixed Gaussian and Lorentzian functions are used to fit D, G, and 2D peaks. FWHM, full width at half maximum.