Skip to main content
Account
Figure 2 | Nanoscale Research Letters

Figure 2

From: Low-density nanoporous iron foams synthesized by sol-gel autocombustion

Figure 2

Room temperature magnetic hysterisis loop of the 600°C-ignited sample. A clear loop can be observed in the VSM result which reveals ferromagnetism of the sample. The saturation magnetization is about 155 A·m2/kg, and the coercivity is about 1.59 kA/m. Inset shows the relationship between saturation magnetization of the prepared sample and the ignition temperature.

Back to article page