Figure 5From: Gas nitriding and subsequent oxidation of Ti-6Al-4V alloysTi-6Al-4V alloy after nitriding at 850°C for 12 h. (a) TEM cross-sectional bright-field image. Selected area electron diffraction patterns of spots (b) 3, (c) 5, and (d) 7.Back to article page