Figure 2From: Investigation of a new lead-free Bi0.5(Na0.40K0.10)TiO3-(Ba0.7Sr0.3)TiO3 piezoelectric ceramicXRD patterns of BNKT-BST ceramics. The samples were sintered at 1,125°C. (a) 2θ = 10° to 80° and (b) 2θ = 44° to 48°.Back to article page