Figure 6From: (Zn,H)-codoped copper oxide nanoparticles via pulsed laser ablation on Cu-Zn alloy in waterTEM BFI and SAED pattern of tenorite in PLA sample after prolonged dwelling in water. Note the slightly preferred orientation of the assembled tenorite nanoparticles in region I to show the (002) and {111} diffraction arcs. The sample was dwelled in water for 20 days after PLA treatment. The Ni counts are from the sample supporting the nickel grid.Back to article page