Figure 6From: Effect of Ag/Al co-doping method on optically p-type ZnO nanowires synthesized by hot-walled pulsed laser depositionThe Arrhenius plots of the exciton bound to the neutral acceptor's PL intensity. (a) 3 and (b) 5 at.% SAZO NWs. Resultant activation energies of the A0X formation are calculated to be about 18.14 and 19.77 meV for 3 and 5 at.% SAZO NWs, respectively.Back to article page