Table 1 Schottky barrier properties of Ag-ZnO contact before and after 400°C annealing

From: Synthesis and electrical property of metal/ZnO coaxial nanocables

Sample

ΦSB(eV)

n

IS(A)

RS(Ω)

As-grown Ag/ZnO nanocables

0.313

1.455

1.004 × 10−10

8.051 × 104

Ag/ZnO nanocable after 400°C annealing in air

0.298

2.686

1.811 × 10−10

1.164 × 105