Table 2 Sun-Voc parameters of the processed solar cells with different Mg thicknesses without an oxidation step
Sample | V oc (mV) | J sc (mA/cm2) | FF (%) | EFF (%) |
---|---|---|---|---|
Mg200 Å | 602 | 36.9 | 80.1 | 17.75 |
Mg300 Å | 598 | 36 | 78.6 | 16.99 |
Mg400 Å | 600 | 35 | 78.4 | 16.67 |
Sample | V oc (mV) | J sc (mA/cm2) | FF (%) | EFF (%) |
---|---|---|---|---|
Mg200 Å | 602 | 36.9 | 80.1 | 17.75 |
Mg300 Å | 598 | 36 | 78.6 | 16.99 |
Mg400 Å | 600 | 35 | 78.4 | 16.67 |