Figure 8From: Room light anodic etching of highly doped n-type 4 H-SiC in high-concentration HF electrolytes: Difference between C and Si crystalline faces3D view using optical profilometry of a sample surface etched during 45 s at 20 mA. The limit between the exposed area where the polishing defects are revealed and the protected one is clearly visible.Back to article page