Figure 10From: 'Wagon-wheel' mask as a tool to study anisotropy of porous silicon formation ratePatterns formed in anodization through a ‘clock’ mask. (а) On a (100) wafer at I = 400 mA and (b) on a (110) wafer at I = 20 mA.Back to article page