Figure 4From: Sputter-prepared (001) BiFeO3 thin films with ferromagnetic L10-FePt(001) electrode on glass substratesDependence of residual strain on sin2ψ for 200-nm-thick BFO films. The films were grown on (a) 20- and (b) 30-nm-thick L10-FePt bottom electrodes at a Td of 400 °C.Back to article page