Table 1 Pore fabrication conditions for PbTe films

From: Abnormal conductivity behavior in porous lead telluride films

Sample number

ja(mA·cm−2)

ta(min)

d(nm)

dpor(nm)

Porosity (%)

1

2

10

510

180

41

2

2

20

790

160

52

3

4

18

440

140

52

  1. ja, anodizing current density; ta, anodizing time; d, thickness; dpor, thickness of the porous layer.