Table 1 OSC at 600 ° C of the CeO 2 , Ce0 .5Zr0 .5O 2 , and Ce0 .5Zr0 .3Al0 .2O1 .9calcined at 1 ,000 ° C for 20 h
Chemical composition | OSC (μmol-O g− 1) |
---|---|
CeO2 | 25.0 |
Ce0.5Zr0.5O2a | 350.0 |
Ce0.5Zr0.3Al0.2O1.9 | 427.0 |
Chemical composition | OSC (μmol-O g− 1) |
---|---|
CeO2 | 25.0 |
Ce0.5Zr0.5O2a | 350.0 |
Ce0.5Zr0.3Al0.2O1.9 | 427.0 |