Chemical composition

OSC (μmol-O g− 1)

Ce0.5Zr0.4Al0.1O1.95

378.0

Ce0.5Zr0.2Al0.3O1.85

389.0

Ce0.5Zr0.1Al0.4O1.8

261.0