Table 2 Summary of triangular microcantilever parameters (SNL and ScanAsyst Fluid) used in LFM study

From: Nanomechanical characterization of chemical interaction between gold nanoparticles and chemical functional groups

 

ScanAsyst Fluid

SNL (B)

L (μm)

70

205

w (μm)

10

40

t (μm)

0.6

0.6

H (μm)

8

8

E (GPa)

304

304

ν

0.24

0.24

θ

60°

64.5°

knorm (N/m)

0.74

0.16

Snorm (nm/V)

12.57

26.30

klat (N/m)

19.57

56.16

Slat (nm/V)

1.88

1.27

  1. L, cantilever length; w, cantilever width; t, cantilever thickness; H, stylus height; E, Young's modulus of Si; v, Poisson's ratio of Si; θ, angle between the base arms of the triangular cantilever; knorm, measured cantilever's normal spring constant; Snorm, measured cantilever's normal sensitivity; klat, lateral spring constant calculated from the knorm; Slat lateral normal sensitivity calculated from Snorm[35, 36].