Table 1 Zeta potentials and pH of GNR, GNR-MUA, and GNR-MUA after adding 30 μL NaOH
From: Induced pH-dependent shift by local surface plasmon resonance in functionalized gold nanorods
Zeta potential | pH | |
---|---|---|
GNR | 58.07 ± 0.55 | 3.92 |
GNR-MUA (0.03 M) | 29.4 ± 0.6 | 7.49 |
GNR-MUA (+NaOH 30 μL) | 8.69 ± 1.3 | 10.16 |