Figure 6From: Optical and microstructural properties of ZnO/TiO2 nanolaminates prepared by atomic layer depositionHigh-resolution TEM images (a, b) of the four-layer ZnO/TiO 2 nanolaminate on Si (100) substrate. Inset shows FFT image of ZnO layer.Back to article page