Figure 3From: Maskless and low-destructive nanofabrication on quartz by friction-induced selective etchingEffect of etching temperature on fabrication efficiency. The etching temperatures were set as 273, 293, 308 and 328 K. The quartz samples were scanned under the same normal load of 8 μN. Dashed lines were fitted by Equation 1.Back to article page