Figure 4From: High-reproducibility, flexible conductive patterns fabricated with silver nanowire by drop or fit-to-flow methodFabrication process of an antenna pattern. (a) Fabrication process of an antenna pattern by drop or fit-to-flow method (inset, the peeled off PDMS). (b) The prepared antenna pattern after being sintered at 125°C for 30 min and 3D image of the conductive track.Back to article page