Figure 12From: The ion implantation-induced properties of one-dimensional nanomaterialsHysteresis loops measure at various temperatures. Hysteresis loops (a) measured at 10 K for Si nanowires Mn+-implanted to doses of 1 × 1015, 5 × 1015, 1 × 1016, and 2 × 1016 cm-2 and (b) taken at 10, 77, and 300 K for Si nanowires Mn+-implanted to a dose of 2 × 1016 cm-2. Reprinted with permission from Wu et al. [61].Back to article page