Figure 4From: Impact of electrically formed interfacial layer and improved memory characteristics of IrOx/high-κx/W structures containing AlOx, GdOx, HfOx, and TaOx switching materialsAFM image of W surface of IrO x /AlO x /W cross-point device. The RMS roughness is approximately 1.35 nm.Back to article page