Skip to main content
Account

Table 1 The LCSTs of Au rod @pNIPAAm-PEGMA nanogels with different molar ratios of NIPAAm/PEGMA

From: Synthesis and characterization of NIR-responsive Aurod@pNIPAAm-PEGMA nanogels as vehicles for delivery of photodynamic therapy agents

NIPAAm (mmol)

PEGMA (mmol)

NIPAAm/PEGMA (mmol/mmol)

LCST (°C)

1.8

0

1:0

32

1.8

0.1

18:1

36

1.8

0.15

12:1

38

1.8

0.2

9:1

40

1.8

0.3

6:1

42

1.8

0.4

4.5:1

44