From: Generation of disk-like domains with nanometer scale thickness in merocyanine dye LB film induced by hydrothermal treatment

Figure 3

The procedure of the hydrothermal treatment (HTT). An aluminum tube (ca. 20 mm in diameter and 150 mm long) was first filled with pure water of 2 mL. The LB sample was put in the tube using a spacer to prevent direct contact of the sample with the water. Finally, the tube was closed by a screw lid using a Teflon tape and immersed in a water bath kept at 80°C.