Figure 2From: Compressibility of porous TiO2 nanoparticle coating on paperboardWater contact angles as a function of the number of calendering nips. For TiO2 nanoparticle-coated and the reference paperboard. The values are taken after 2 s of the droplet application on the surface.Back to article page