Figure 1

XRD patterns of the samples. (a) x%Zr/N-TiO2(500), x = 0.1, 0.3, 0.6, 1.0, 5.0, 10; (b) samples of 0.6% Zr/N-TiO2 calcined at 400°C, 500°C, and 600°C.
XRD patterns of the samples. (a) x%Zr/N-TiO2(500), x = 0.1, 0.3, 0.6, 1.0, 5.0, 10; (b) samples of 0.6% Zr/N-TiO2 calcined at 400°C, 500°C, and 600°C.