Table 1 BET surface areas of the x%-Zr-N-TiO 2 -500 samples with different Zr doping concentration calcined at 500°C
Samples ( x%-Zr-N-TiO2-500) | Surface areas (m2g−1) |
---|---|
0.1 | 122.31 |
0.3 | 142.96 |
0.6 | 143.04 |
1.0 | 166.25 |
5.0 | 218.18 |
10.0 | 240.18 |
Samples ( x%-Zr-N-TiO2-500) | Surface areas (m2g−1) |
---|---|
0.1 | 122.31 |
0.3 | 142.96 |
0.6 | 143.04 |
1.0 | 166.25 |
5.0 | 218.18 |
10.0 | 240.18 |