Figure 2From: Pulsed laser-induced formation of silica nanogridsInfluence of confinement. Patterned 150-nm-thick SiO x film irradiated (a) without and (b) with confinement (after peeling off the confinement layer); laser parameters: 248 nm, 260 mJ/cm2, 1 pulse.Back to article page