Table 1 Variation in peak intensities measured from XRD diffractograms of ultrathin (15 nm) ZnO NW arrays
ZnO peak | 300 K (room temperature) | 473 K | 673 K | 873 K | ||||
---|---|---|---|---|---|---|---|---|
Intensity | Relative intensity | Intensity | Relative intensity | Intensity | Relative intensity | Intensity | Relative intensity | |
100 | 190.0 | 0.24 | 254.1 | 0.39 | 264.9 | 0.4 | 279.2 | 0.47 |
002 | 211.5 | 0.26 | 254.0 | 0.45 | 346.9 | 0.63 | 357.9 | 0.68 |
101 | 342.5 | 0.64 | 451.1 | 0.72 | 530.9 | 0.85 | 569.9 | 1.22 |