Skip to main content
Account

Table 2 Variation in peak intensities measured from XRD diffractograms of thin (100 nm) ZnO NW arrays

From: Tuning of structural, optical, and magnetic properties of ultrathin and thin ZnO nanowire arrays for nano device applications

ZnO peak

300 K (room temperature)

473 K

673 K

873 K

Intensity

Relative intensity

Intensity

Relative intensity

Intensity

Relative intensity

Intensity

Relative intensity

100

114.7

0.02

155.1

0.03

257.4

0.1

312.1

0.13

002

119.4

0.03

162.7

0.06

248.8

0.07

261.8

0.11

101

264

0.03

389.8

0.06

460.0

0.25

623.6

0.26

Navigation