Figure 3From: Enhanced resistive switching memory characteristics and mechanism using a Ti nanolayer at the W/TaO x interfaceAFM image for surface roughness. The surface roughness of 200-nm-thick W layer on SiO2/Si substrate is approximately 2.8 nm.Back to article page