Table 1 R sq of spray-coated Ag patterns based on various sintering operations
From: Spray-coated nanoscale conductive patterns based on in situ sintered silver nanoparticle inks
Temperature | R sq | Time | R sq | Time |
---|---|---|---|---|
(°C) | (post sintering) | (post sintering) | (in situ sintering) | (in situ sintering) |
(Ω/sq) | (s) | (Ω/sq) | (s) | |
140 | 20.6 | 320 | 6.1 | 52 |
150 | 6.3 | 260 | 4.6 | 40 |
160 | 3.3 | 120 | 2.2 | 28 |
170 | 1.4 | 50 | 1.8 | 20 |
180 | 1.2 | 35 | 1.4 | 16 |
190 | 1.0 | 20 | 1.4 | 15 |
200 | 0.94 | 17 | 1.1 | 15 |