Table 2 Percent change in sheet resistance after the tape test on differently prepared electrodes
From: Hot-rolling nanowire transparent electrodes for surface roughness minimization
As-deposited | Annealed | Rolled at 80°C | |
---|---|---|---|
Sheet resistance change after tape test | Open circuit | 510% | 0.9% |