Table 1 Doping concentration of Sn in ITO NPs measured by XPS spectra and ICP-AES

From: Tunable surface plasmon resonance frequencies of monodisperse indium tin oxide nanoparticles by controlling composition, size, and morphology

Initial Sn concentration (at %) ([Sn]/([Sn] + [In])

Sn doping

Concentration (at %)

XPS

ICP-AES

6.0

5.8

5.9

7.6

7.3

7.3

10

10.3

9.5

12

11.4

11.5