Figure 4From: Improving the efficiency of cadmium sulfide-sensitized titanium dioxide/indium tin oxide glass photoelectrodes using silver sulfide as an energy barrier layer and a light absorberXRD pattern of the CdS(1) /Ag 2 S /TiO 2 /ITO film. XRD pattern of the CdS(1)/Ag2S/TiO2/ITO film (a) for 2θ between 10° and 80° and (b) for 2θ between 23° and 52°.Back to article page