Figure 3From: Synthesis of flake-like graphene from nickel-coated polyacrylonitrile polymerFE-SEM images of the Ni-coated PAN films after the pyrolysis at 950°C/10 min. Where the coated Ni thickness is 40 nm (a), 100 nm (b), and 200 nm (c), respectively.Back to article page