Table 1 Activation energy of conductivity on the concentration NPs in glassy phase of nanocomposites along and across cation-anion layers

From: Influence of semiconductor and metal nanoparticles on the dielectric properties of ionic matrix cadmium octanoate

Concentration of NPs in samples

Pure CdC8

2% CdS

4% CdS

6% CdS

2% Au

4% Au

4% Au  +  2% CdS

Е ║, eV

0.017

0.015

0.013

0.003

0.33

0.16

0.009

Е , eV

0.04

0.027

0.023

 

0.16

0.1

0.18