Table 3 Dependence of the anisotropy of the conductivity on the concentration of CdS and Au nanoparticles

From: Influence of semiconductor and metal nanoparticles on the dielectric properties of ionic matrix cadmium octanoate

Concentration of NPs in samples

Pure CdC8

2% CdS

4% CdS

2% Au

4% Au

4% Au +  2% CdS

AG

17.5

44

68.3

12.3

17.1

5.7

AS

125

110

69

57.3

33.6

43.2

  1. AG, anisotropy of the conductivity for the glassy phase; AS, anisotropy of the conductivity for the smectic phase.