Figure 5From: The impact of thickness and thermal annealing on refractive index for aluminum oxide thin films deposited by atomic layer deposition Annealing temperature dependence of refractive index for ALD-Al 2 O 3 with different thicknesses. (a) 50 cycles, (b) 100 cycles, (c) 300 cycles, and (d) 500 cycles.Back to article page